Abstract

Phase relations within the system Fe–Nb–S were studied experimentally by the technique of evacuated silica glass tubes in the temperature interval 400–1000°C. The dominant field in the system is a broad solid-solution FexNbyS2 (0 < x < 0.5, 1.0 < y < 1.4) that includes the composition of the mineral edgarite. Also, it forms stable assemblages with pyrrhotite and pyrite. The iron sulfides dissolve limited amounts of Nb: pyrrhotite dissolves up to 1.13 at.% Nb, and pyrite, only 0.02 at.% Nb. We refined the crystal structure of five samples of the FexNbyS2 solid solution, and established the relation between the unit-cell volume and Fe/(Fe + Nb). The occurrence of edgarite can be expected in associations with other sulfides crystallizing under extremely low fugacity of oxygen.

Abstract

Nous avons étudié expérimentalement les relations de phases au sein du système Fe–Nb–S en utilisant des tubes de verre siliceux évacués, sur l’intervalle 400–1000°C. La solution solide FexNbyS2 (0 < x < 0.5, 1.0 < y < 1.4) occupe un champ de stalilité dominant qui comprend la composition du minéral edgarite. De plus, ce minéral peut former des assemblages stables avec la pyrite et la pyrrhotite. Les sulfures de fer peuvent dissoudre des quantités limitées de Nb; la pyrrhotite peut dissoudre jusqu’à 1.13% Nb (proportion atomique), et la pyrite, seulement 0.02%. Nous avons affiné la structure cristalline de cinq échantillons de la solution solide FexNbyS2, et établi la relation entre le volume de la maille et Fe/(Fe + Nb). On peut s’attendre à trouver l’edgarite en association avec d’autres sulfures à des conditions de fugacité d’oxygène extrêmement faibles.

(Traduit par la Rédaction)

You do not currently have access to this article.